Gelcoat Gun Nozzle Size


Author
Message
Brian_s
Brian_s
Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
I printed a new Nozzle. I have not had a chance to try it yet. I bought a HVLP spray gun with a 3mm nozzle. Seems to work OK but it is more fiddly to clean.

http://i1269.photobucket.com/albums/jj586/BrianSaville/DSCF0815.jpg 
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
It's wonderful for gelcoating something this size:

https://fbcdn-photos-c-a.akamaihd.net/hphotos-ak-xfa1/v/t1.0-0/10917125_600966583368095_5689629948276944711_n.jpg?efg=eyJpIjoidCJ9&oh=d5c8448a3ccd1e44ded6ef6b7bddabb7&oe=56207BF6&__gda__=1448321472_7bf14a0e7ca77e874daa08aaaf640981


That would have been impossible to do by brush and a nightmare to do with a HVLP gun. The G100 got it done quick and easy. 
George Sychrovsky
George Sychrovsky
Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)
Group: Forum Members
Posts: 24, Visits: 1.6K
I have this gel coat gun and its horrible piece of tool
I use harbor freight gun with 2.2 mm tip but I thin the gel-coat with some styrene or acetone


---------------------------------------------------------------------
Disclaimer opinions of others will vary depending on what they are selling
AdamHutchin
AdamHutchin
Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)
Group: Forum Members
Posts: 8, Visits: 53
I first of all just went for a cheapo eBay special, I wanted to make sure it would actually work before investing in a better gun.

If you're looking at a "decent gun and compressor setup", I'd say always get the biggest compressor you can afford.  Air tools like belt sanders etc are really useful for composite work but can use a lot of air.  I've got a 100L, 3HP unit and it's big enough to spray/run air tools etc quite happily, fairly constantly.  I used to have a smaller 30L one and it was largely useless.  It just couldn't keep up.  Hanaldo makes some good points about cleaning though, the 1.8 tip is no fun for that!

Hanaldo, I do have a depth gauge, I just happened to be spraying it into a mould with lots of curvature in it.  the variation in thickness just came from my inexperience of using the gun and I ended up with thicker areas in some of the tighter radii than others.  I just need to practice and be less cack-handed. Smile
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
The cheaper guns often have rubber seals in them that will melt when exposed to the gelcoat/acetone. So it's better to buy a good quality one; note that doesn't necessarily mean more expensive! Best bet is to ask for something that can handle acetone at a spray paint supply store or similar. 

Also if you can, get a bigger tip. 2.5-3mm is ideal. Smaller will work, but it's harder to clean and you don't need to worry about orange peel from the bigger tip. 

Adam, I do recommend buying a gelcoat depth gauge if you're having trouble with the thickness. It can make quite a difference if your gelcoat is sensitive to thickness (which many are), so it's good to have a tool to measure it until you get the feel for it. And they are cheap cheap, so it's a no-brainer really. 
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
what make of spraygun did you go for? Would the cheaper all in one HVLP systems be of use or is it worth going the full hog and buying a decent gun and compressor setup?
AdamHutchin
AdamHutchin
Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)
Group: Forum Members
Posts: 8, Visits: 53
I thought I would reply to this as it's a question I'd been trying to find the answer to previously.

I didn't want the EC cup gun as it seems to be designed for delivering loads in much higher quantities than I was looking for, like you I wanted to do a comparatively much smaller mold.

In the end I just used a normal spray gun with a 1.8mm tip and it worked really well.

I would suggest though that you actually look at the gun before buying one as I went into a shop and took two of them apart.  One of them would have been a nightmare to clean all the gel coat out of whereas the other is much more straight forward; still not a fun job but manageable.

The other thing I found is that it's quite hard to visually gauge the thickness of a clear gel coat as you're spraying it.  Even with a 1.8mm nozzle I still ended up spraying it too thickly in some places but I guess with some practice it will become easier.
Brian_s
Brian_s
Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
I hadn't thought of that. I will give it a try.

Thank you.

Brian.
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Very clever!

Can you use the 3d printer to make a smaller nozzle for the gun? 😉
Brian_s
Brian_s
Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)Supreme Being (791 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K

This is a picture of one of my Moulds.

http://i1269.photobucket.com/albums/jj586/BrianSaville/DSCF0742.jpg

As you can see it is not very wide but it is long.

I made a modification to the cup gun. I usually only spray about 100g of GC50 which is about enough to wet the cup. I used a 3D printer to make an adaptor to fit a smaller cup. It works quite well.

http://i1269.photobucket.com/albums/jj586/BrianSaville/DSCF0743.jpg

http://i1269.photobucket.com/albums/jj586/BrianSaville/DSCF0744.jpg
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search