Hi,

I'm Mike, from Leeds, UK.

I'm a kind of project guy. A very keen racing cyclist and motorbiker, interested in developing my skills in carbon fibre parts manufacture and CF repair work.

Really interested to know about how to bond inserts into mouldings, like say, screw thread adapters and studs so my mouldings can be fastened into place....as well as just making really cool stuff.

I'll be reading this forum to learn and contribute my tales of success and ..... not success!

Mike
davro
davro
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Hi Mike,

Looking forward to seeing your creations Smile



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
welcome! a "not succes" is part of the way to go to "succes" so dont be ashamed to ask some questions when failing Smile sure you will be helped by many of us who has gone the same way 

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Hi Mike,
Like you i like a bike or 2 or 3, haha.
welcome, hope you post some of your work up.

Chris.
Jacopo Carbonio
Jacopo Carbonio
Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)
Group: Forum Members
Posts: 43, Visits: 109
Welcome Mike w00t
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi Mikebike
Welcome to the forum . I am also a bike fan must it must have an engine fitted Smile
Chris 
Carbon fibre works LTD

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Mikebike
Mikebike
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 13
Cheers everyone! I feel very welcome.

I've been blasting through my fabric and resin running trials and getting somewhere, to the point where I'm now proudly riding my Daytona with its carbon rear hugger and heel guards.....even though they're not perfect. A mate couldn't believe I'd made them.



I'll post some pics soon. They look really nice when finished with a satin or matte lacquer. Dull, but bling at the same time.

The best fun has been designing ejector screws into my moulds and hearing the release crackle as the part ejects, without having to be levered out by hand.

Next steps.....new EC mould putty, EC vac bag kit, vac pump (which I found for £60, phew!) to make some fuel tank surrounds. 
Mikebike
Mikebike
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 13

Here's the latest parts
Attachments
image.jpg (529 views, 1.00 MB)