Darren
Darren
Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)
Group: Forum Members
Posts: 54, Visits: 916
this is the second attempt at this part, same problem each time, seems to have dry ares or air voids.
Any advice would be great, cheers


Replies
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Lets say I switch to infusion, how many layers of CF will it penetrate?


Baja Patient is right, the resin will go through as many layers as you have in your laminate. Resin flows well through woven reinforcements (particularly twill weaves). I've never known a laminate too thick to infuse.

In places the thickness will be 5-7 mm, will infusion penetrate all those layers of CF? (some UD fibers in there also.)


The UD fibres won't infuse very well; they sit so tightly packed that the resin would find it difficult to get through. If you're using unidirectional carbon with infusion then you should use UD that has some weft (i.e. it is 90% UD with some glass or carbon running the opposite way, like a woven fabric but with the vast majority of the fibre running lengthways. UD in this format is particularly common as a tape (a strip of woven material between 100mm and 500mm).

I guess the answer is yes with the corrects routing and blocking of the feed, in that case is that expert stuff that I should practice until perfection, or straight forward?                                                    


Well, making a structual subframe itself is certainly not basic/beginner work but if you've designed it correctly, the actual infusion should not really present any problems that would not be encountered when infusing something less ambitious.

All the best with it,

Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
prsw
prsw
Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Darren - 14 Years Ago
Warren - 14 Years Ago
Darren - 14 Years Ago
Shaneer22 - 14 Years Ago
Paul (Staff) - 14 Years Ago
prsw - 14 Years Ago
Matt (Staff) - 14 Years Ago
prsw - 14 Years Ago
Matt (Staff) - 14 Years Ago
                                 Thank you.
prsw - 14 Years Ago
Leon - 14 Years Ago
prsw - 14 Years Ago
baja_patient - 14 Years Ago