flamypie
flamypie
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 9,
Visits: 45
Hi there, hopefully you can point me in the right direction.
I need to make a copy of this mount currently made from plastic. Im simplifying the shape and making a small mould so what I need to know is if casting resin would be a suitable material to replicate it in being that it would be solid resin and then bonded to an epoxy pre preg part. Please see picture of the mount below and to give an indication of the size it is 25mm x 25mm approx.
Thanks in advance
Reply
Like
4
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
I've tried to do this before, but the casting resin wasn't strong enough to be used successfully as a mount.
My advice is to use a rivnut instead.
Reply
Like
4
flamypie
flamypie
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 9,
Visits: 45
I can see what your saying. I have been giving it a good look over this morning and I think in going to make a normal carbon piece for the bottom section then bond a piece of nylon to screw into. I have never used casting resin before and thought I may be able to achieve a plastic moulded looking part when using it.
It was worth asking the question.
Many thanks
Reply
Like
5
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Yeh I followed the same train of thought when I first started dealing with parts with fasteners like that.
These days I follow a different approach, keep it simple. The simplest solution is generally always the best solution.
Reply
Like
5
ChrisR
ChrisR
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
you could make the part to bond into the main section from polyurethane casting resin rather than epoxy, fix a rivnut/threaded insert into the mould before casting
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search