Hello all,

I was looking at the new flexible epoxy of easycomposites. Could this be used to create a flexible product which when bent would flex and then return back to its original shape? Like for example a dirt bike fender. 

Alao, how would you select the materials? 2 layers of CF? The product wouldn't need to be very strong, more cosmetic and covering. 

Lastly, is the flexible epoxy UV resistant? If not, is there a good coating that won't crack if flexed?

Thank you in advance.
Reply
Wabba
Wabba
Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)Supreme Being (217 reputation)
Group: Forum Members
Posts: 21, Visits: 64
Thank you for that Matt, much appreciated.

That is good news about the 1kg size. Once I get the plug/mold done I'll give this a try.

Best regards
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search