Hi

I am trying to bond a small piece of flat 2mm pre oreg carbon fibre to the side of a 5mm diameter carbon fibre rod and want to know what the strongest possible bonding method I should use.

The part once finished will have daily force put on it so really needs to be super strong.
I am considering using the ET-500 adhesive but not sure if that would be strong enough.

Any advice?

Thanks
Aysar
Dravis
Dravis
Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
EC VM100 Vudu Glu ... 

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As Dravis said, VuduGlu™ VM100 Black is a great choice.  However if you need something with less odour then our PT326 20min Rigid Polyurethane Adhesive Twin Tube is a very good alternative.

Remember to give both surfaces a good key and degrease to achieve the best bond.  Also where the bonding surface area is small, it can help to use "fillets" of adhesive to increase the bonding surface area and hence bond strength.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Dravis
Dravis
Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I like the smell of "vudu glu"  LaughBigGrinWow

One advantage of Vudu Glu is that you can buy it in a small 25 gram syringe.. PT326 only comes it the 50 gram "twin tube"
I'm still on my first "twin tube" of PT326 ...  Whistling

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Aysar
Aysar
Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)
Group: Forum Members
Posts: 3, Visits: 16
Thanks everyone.

I have ordered the vudu glu and shall be testing it.

Thanks

Aysar
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search