Hi all,

I have made a few parts which have a few pin holes, whats the best/easiest method for removing these, do you just mix a bit of resin with fast hardener and keep applying until the hole is filled and then flat off or is there a better method? 

cheers
Lee.
Reply
morepower
morepower
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
With out of autoclave pre-pregs getting better there is less need for an autoclave for almost all the work we as either small businesses or hobbyists do. The added strength given is not that great so adding one more layer or not making a part that is quite so structural is the compromise. How many meters of material would we need to use to make the cost of the autoclave worth while? 

The one thing that does seem important is the ramp and dwell controller for OOA's. I know some get great results without one but having one does take out human error where the oven is concerned. Plus the cost of a controller is only a small one which could be paid for with one or two items that fail due to user error. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Toffee - 10 Years Ago
Hanaldo - 10 Years Ago
Toffee - 10 Years Ago
f1rob - 10 Years Ago
flamypie - 10 Years Ago
Bonobo - 10 Years Ago
scottracing - 10 Years Ago
f1rob - 10 Years Ago
f1rob - 10 Years Ago
morepower - 10 Years Ago
MarkMK - 10 Years Ago
morepower - 10 Years Ago
scottracing - 10 Years Ago
20_rc51_00 - 10 Years Ago
morepower - 10 Years Ago
sam - 10 Years Ago
sam - 10 Years Ago
MarkMK - 10 Years Ago
morepower - 10 Years Ago
MarkMK - 10 Years Ago
morepower - 10 Years Ago
ArturK - 9 Years Ago
morepower - 9 Years Ago
Hanaldo - 9 Years Ago
morepower - 9 Years Ago
Hanaldo - 9 Years Ago
morepower - 9 Years Ago
scottracing - 9 Years Ago
Hanaldo - 9 Years Ago
Hanaldo - 9 Years Ago
TomDesign - 9 Years Ago
Hanaldo - 9 Years Ago
TomDesign - 9 Years Ago
Hanaldo - 9 Years Ago
morepower - 9 Years Ago
TomDesign - 9 Years Ago
morepower - 9 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search