Now thats the other side of DIY, That's one fancy pump!
Just today I used my new catch pot gotta say I like that I can store pressure in it, Just like you said in a leak detecting situation dont wanna have that pump on.
now I seal the mould off from the pot and if the bag gets to loose while im fingering my mould, I can open the valve for a sec and suck it back to 30 psi from the tank.
I can almost do a complete resin pull just with the pressure in the tank haha!