Can anyone explain how to get a perfect join in 2 pieces of carbon fibre material when doing carbon fibre skinning?
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
2" is normally the recommended overlap. 

You will barely notice the overlap with only 3 layers, even if they are vertical. It's on the back side anyway, so I'm not sure why that would be an issue unless you need a cosmetic B side as well? 