50mm/2" is about right.  In theory, you should stagger the joint but in practice for most panels it makes little difference as the additional thickness in that area will mostly compensate for the joint.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
2" is normally the recommended overlap. 

You will barely notice the overlap with only 3 layers, even if they are vertical. It's on the back side anyway, so I'm not sure why that would be an issue unless you need a cosmetic B side as well? 
Trevor Harris
Trevor Harris
Supreme Being (267 reputation)Supreme Being (267 reputation)Supreme Being (267 reputation)Supreme Being (267 reputation)Supreme Being (267 reputation)Supreme Being (267 reputation)Supreme Being (267 reputation)Supreme Being (267 reputation)Supreme Being (267 reputation)
Group: Forum Members
Posts: 22, Visits: 116
Hi Warren,

                 When using the infusion process for max strength how much overlap is needed on carbon twill fabric on adjoining sheets? If the stack is say three layers thick should the joints be staggered so they are not in alignment verticaly?

Trevor
Dravis
Dravis
Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Yep ... If the part you want to skin does not have too much compound curvature, then Pro-finish cut with very sharp scissors (Like EC's CF/kevlar ones) is the way to go.

When skinning, overlapping the edge can sometimes leave a ridge, so I try to lay it "edge to edge" even though it takes a lot of careful handling-

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The best way is to use our ProFinish Carbon Fibre 2/2 Twill as you can cut neat edges with little or no fraying.  We always recommend the second sheet overlaps the edge of the first so you don't get any gaps.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Timellis
Timellis
Supreme Being (186 reputation)Supreme Being (186 reputation)Supreme Being (186 reputation)Supreme Being (186 reputation)Supreme Being (186 reputation)Supreme Being (186 reputation)Supreme Being (186 reputation)Supreme Being (186 reputation)Supreme Being (186 reputation)
Group: Forum Members
Posts: 14, Visits: 58
Can anyone explain how to get a perfect join in 2 pieces of carbon fibre material when doing carbon fibre skinning?