Thought as these tools are pretty much hand made by each laminator for laying up prepreg, but you cant find much info on them I would post up a pic of some of mine. I'm in the process of making some new ones as I haven't been able to bring my toolbox to germany yet and I've got some parts to make soon.
So heres mine, no doubt some of the more 'unusual' prodders will make an appearance if any of the lammys want to share them Smile


Attachments
20150326_161115_resized.jpg (1.5K views, 1.00 MB)
Reply
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Teflon tools for me too. mine are a 10mm thick sheet cut into various shapes to suit your preference. Nice and slippery on the carbon too.