Help removing plug from mold!


Author
Message
dbayton
dbayton
Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)
Group: Forum Members
Posts: 2, Visits: 52
Ok so I made a two part mold of an auto body panel. The top released fine as it was a normal metal body panel. The bottom however did not release. The backside is metal coated with a very hard paint type coating. I used two thick coats of pva, but that's it. I already know I should have used wax, or just a better release agent completely. In any event, now I have a plug stuck in the mold.

I'm going to try soaking it in hot water tonight, and I was going to try heating the back with a heat gun as well. Any other ideas? Worse case would be to cut the mold off of my plug, but that would obviously ruin all of my hard work. The pva didn't do a great job, but I don't believe the tooling gel made a solid bond to my plug either. So I think it will come off with enough work.

Any ideas or advice from any of you more experienced guys?
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
If you have access to an air compressor ? an air injected wedge might work if you can get it in there Wink
Helps air to be forced between the mould and the plug ...





David Stevens
YouTube: Comment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


dbayton
dbayton
Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)
Group: Forum Members
Posts: 2, Visits: 52
I went to Harbor Freight yesterday specifically looking for an air wedge tool like that, and I couldn't find one. I know I could order one online, but i'm looking for a more immediate solution. Do you know of any brick & mortar stores that sell an air wedge?
kidpaint
kidpaint
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 99, Visits: 676
if you have any access to a small opening to get a rubber tipped blow gun into that usually does the trick. I often just use a blow gun and a wooden wedge. I get the wedge started and then blow air down in between. Worse case so far Ive use a rubber mallet and lightly as to now ruin anything tapped around the part to get it to help release as a buddy pulses the air into it. 
Brian2fast
Brian2fast
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 79, Visits: 1.3K
I'd also go with wooden wedges. I used oak to make nice thin but long wedges, then rubbed candle wax all over it. They didn't mark my carbon part that was stuck in its mould and I was being pretty ruthless with the hammer driving the wedge in.

Craig