By dbayton - 4/13/2015 7:54:29 PM
Ok so I made a two part mold of an auto body panel. The top released fine as it was a normal metal body panel. The bottom however did not release. The backside is metal coated with a very hard paint type coating. I used two thick coats of pva, but that's it. I already know I should have used wax, or just a better release agent completely. In any event, now I have a plug stuck in the mold.
I'm going to try soaking it in hot water tonight, and I was going to try heating the back with a heat gun as well. Any other ideas? Worse case would be to cut the mold off of my plug, but that would obviously ruin all of my hard work. The pva didn't do a great job, but I don't believe the tooling gel made a solid bond to my plug either. So I think it will come off with enough work.
Any ideas or advice from any of you more experienced guys?
|
By Brian2fast - 4/18/2015 4:26:20 PM
I'd also go with wooden wedges. I used oak to make nice thin but long wedges, then rubbed candle wax all over it. They didn't mark my carbon part that was stuck in its mould and I was being pretty ruthless with the hammer driving the wedge in.
Craig
|
|