3 Section Sea Kayak ( Resin Infusion ) ?


Author
Message
Andrew Swingler
Andrew Swingler
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 2, Visits: 7
Hello Guys,

I have made a 3 section sea kayak male mould from timber. ( Bow - Cockpit - Stern ) and have sealed the timber with polyester resin.

My question is. Is it possible to resin infuse a male mould as the outer part of the mould will be the interior of the kayak and the outer part of the kayak will have the vacuum bagging on it. Will the outer be a total mess or can this be overcome by skinning. I was going to use black Diolen 2/2 twill fabric with 2mm Lantor Soric. Any body have any ideas.

Andrew
panda
panda
Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)
Group: Forum Members
Posts: 47, Visits: 2.1K
at,You could do it this way but i find it much harder seaming the inside of the kayak once out the mold.  I would make a female mold off what you have and the build the sections in that.  Bolt the sections together and seam the inside then release from the mold.  Far less work getting a good finish on the final part if it is straight from the mold.

Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I agree with Panda on this. That would be a much easier technique in terms of getting a good outer finish.

Also be aware that Epoxy and Polyester can cause some issues especially when using wet epoxy on a polyester mould. Generally we advise avoid doing it to avoid chance of part sticking.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Andrew Swingler
Andrew Swingler
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 2, Visits: 7
Thanks Panda and Warren for your comments. You've given me something to think about now.

Andrew
panda
panda
Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)
Group: Forum Members
Posts: 47, Visits: 2.1K
I have several molds for kayaks if you need any pictures of them, normally its a deck mold, hull mold and a cockpit mold. 