Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Carbon Fibre Cloth Fabric
»
Profinish Carbon Cloth Storage
Profinish Carbon Cloth Storage
Post Reply
Like
9
Profinish Carbon Cloth Storage
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Suika
Suika
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 21
I know that Pre-Preg Carbons generally have a "shelf life", and since the Profinish cloth has a resin binder on one side of the cloth, does this mean that it too will have a shelf life? Should it be stored in a freezer to extend the life of the product?
Tags
Profinish
Profinish Storage
Reply
Like
9
Brian_s
Brian_s
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 99,
Visits: 2.5K
No. The binder is set and needs no special storage. It is just a fine spray to hold the weave together.
Brian.
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search