By Suika - 4/4/2015 12:32:41 AM
I know that Pre-Preg Carbons generally have a "shelf life", and since the Profinish cloth has a resin binder on one side of the cloth, does this mean that it too will have a shelf life? Should it be stored in a freezer to extend the life of the product?
|
By Brian_s - 4/4/2015 9:11:21 AM
No. The binder is set and needs no special storage. It is just a fine spray to hold the weave together.
Brian.
|
|