Profinish Carbon Cloth Storage


Author
Message
Suika
Suika
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 1, Visits: 21
I know that Pre-Preg Carbons generally have a "shelf life", and since the Profinish cloth has a resin binder on one side of the cloth, does this mean that it too will have a shelf life? Should it be stored in a freezer to extend the life of the product?
Brian_s
Brian_s
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
No. The binder is set and needs no special storage. It is just a fine spray to hold the weave together.

Brian.