Group: Forum Members
Posts: 107,
Visits: 504
|
i'm guessing that it would have material on the bottom aswell?
i would make the mould in 3 pieces 1 on the left and 1 on the right as if it was a 2 piece mould (like you were thinking) then 1 on the bottom that way when you come to lay the fabric inside, you can leave off the bottom section and gain access to the rest of the mould with pro-finish carbon to get the visual effect, then bolt the bottom piece on and carry on laying up.
|