This guitar neckuses Carbon fiber as an exoskeleton with a lightweight wood core, such aswillow or basswood as a compression medium for the core. The finalouter face of the neck is a thin 1/32” veneer of hard wood. Therecan be as much as 200 pounds of pull on a guitar neck.

I've attached my design


Myquestion is do I have the design right? Where can it be improved?


Attachments
3D Neck Post..pdf (499 views, 91.00 KB)
12th fret profile..pdf (449 views, 79.00 KB)
Reply
Eldon H
Eldon H
Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)
Group: Forum Members
Posts: 6, Visits: 25
Yes ,No truss Rod. Well I hope.

Attached is a previous attempt at this without a truss rod.

Here I simply hollowed out a guitar neck and added carbon and a willow core.

After six months of use this neck is bowing a little more than anyone would like.

Per the previous post.  This might be because I did not complete the carbon Box on the top of the neck?

Also I now believe that the vertical carbon in the center is use less.

I am open to all suggestions.
Attachments
DSC08808.JPG (414 views, 3.00 MB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search