Composite Guitar Neck, I need Help with the design.


Author
Message
Eldon H
Eldon H
Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)
Group: Forum Members
Posts: 6, Visits: 25
Yes ,No truss Rod. Well I hope.

Attached is a previous attempt at this without a truss rod.

Here I simply hollowed out a guitar neck and added carbon and a willow core.

After six months of use this neck is bowing a little more than anyone would like.

Per the previous post.  This might be because I did not complete the carbon Box on the top of the neck?

Also I now believe that the vertical carbon in the center is use less.

I am open to all suggestions.
Attachments
DSC08808.JPG (550 views, 3.00 MB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search