			            After pressure bagging, I have some "pin-pricking" in the final surface. I've played around now with a couple of shots at different pressures, but it doesn't make a lot of difference to the outcome. 
  What's a good way of closing it up ? I don't REALLY want to fill, and then sand them up and repolish......
  Steve                
			            				
			                                 
                     
                                            
                         
                    
                  
             |