Our PT326 or VM100 will technically bond them together very well in a structural sense, however both glues are black/dark charcoal.
You would be better off using some of the waterclear resin itself as an adhesive. Key and clean both surfaces then apply a thin layer of mixed resin and press together and clamp until cured.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|