Many thanks Warren.

Regards
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Our PT326 or VM100 will technically bond them together very well in a structural sense, however both glues are black/dark charcoal.

You would be better off using some of the waterclear resin itself as an adhesive.  Key and clean both surfaces then apply a thin layer of mixed resin and press together and clamp until cured.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Ray Rogers
Ray Rogers
Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)
Group: Forum Members
Posts: 18, Visits: 79
What glue should I use for fixing 2 Water Clear Polyurethane Casting resin together please?