Boat builders, chandlers, canoe places, car body places etc all likely to supply composite materials and hence a usable MEKP.
There is nothing special about the MEKP we supply, you can ask at your local supplier for ‘Standard reactivity MEKP’; brands such as Andanox KP9, Akperox A30, Butanox M50 (Akzo Nobel) are all suitable and very widely available.