  I had a demand from a client that wants me to produce a kevlar panel with a specific thickness, so..
  Desired thickness is 8mm using the 300gsqm which as a thicknes of 0.47mm
  Using epoxy resin and vacuum bagging, how many layers of kevlar do I need to achieve the client desired thickness of 8mm?
  Btw, how to calculate the needed amount of resin to this?
  the exact dimension are: 2780mm x 710mm x 8mm (Yep, huge!!!!).
  Can someone help me with this?                
			            				
			                                 
                     
                                            
                         
                    
                  
             |