What is the smallest radius corner you can successfully vacuum bag carbon finer around? 
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Depends on the cloth. The thicker the cloth, the harder to conform to right radii.  With the addition of vacuum and careful manipulation you should be able to force the carbon around most tight corners, however the risk of it going wrong is higher the tighter the corner.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant