Hi, 
I bought epoxy infusion resin in late 2012/early 2013 but due to my daughter becoming unwell haven't had an opportunity to use it til now, will the resin still cure and be strong? 
Thanks, 
Donnacha. 
Reply
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
The polyamine hardeners are usually light sensitive.  They can be stored longer in the dark.  They will darken and still be good but as brainfart says if they have gone solid then they are well past it.