Talk Composites - The Forum for Advanced Composites
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
infusion resin shelf life?
http://www.talkcomposites.com/Topic14029.aspx
By SakerProject
-
12/1/2014 10:37:57 PM
Hi,
I bought epoxy infusion resin in late 2012/early 2013 but due to my daughter becoming unwell haven't had an opportunity to use it til now, will the resin still cure and be strong?
Thanks,
Donnacha.
By SakerProject
-
12/2/2014 8:22:50 PM
Thanks for the replies and advice, I'll definitely take it on board, Donnacha.