Hi
Until now I have been using epoxy resin to infuse my parts at home but I now have the chance to use Crestapol 1250LV urethane acrylate resin which is the system we use at work. My question is will this be compatible with the pro finish CF that is partially impregnated with a resin polymer?
I've asked easy comp's but as yet have no answer, I presume because its not a resin that's in everyday use. Does anyone here know?
Reason I want to use it is that IMO its a better resin that's cheaper and gives a more flexible / resilient product which is perfect for larger infusions like bumpers, the cure time can be changed from a standard 2hr's to 5 mins and the viscosity can be changed with heat to get a better flow on more complex parts.
Any help would be greatly appreciated.
|