Hi,

I am pondering a new boat build which will, in all eventuality, comprise making the hulls (it's a catamaran), foils, beams and maybe even a mast. I am pretty impressed with the Easy-preg option for an off the mould finish, ready for paint directly - I don't want the weight penalty of a gel coat if possible. The hulls would be a Nomex sandwich and I assume that this would be OK with a 215 gsm vari-preg layer (don't want to go to the 430 or would the experts recommend a resin layer? If so, where do I get this as there is nothing on the Easy Composites site that looks like it fits the bill. I'd like to work on a single vacuum / over cure rather than doing curing the layers individually.

My second train of thought is how to incorporate UD layers in the vari-preg system. The cat's beams, foils and mast will be a UD dominated laminate, so I will need to work this out! Again, is there sufficient resin within the vari-preg backing layer to co-infuse UD layers, or again will a resin layer be required?

Got to build an oven of course, but I'd like to get the construction resolved in my head at least.

Thanks for the great tutorials.

Cheers

Andy
Replies
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
> this would be OK with a 215 gsm vari-preg layer

You want to build a boat with only one layer of 215g as sandwich skins? This will not provide sufficient strength unless used in a small RC model. This might be barely sufficient for an aircraft traveling through air, but certainly not for a boat going through a dense medium like water if this boat is supposed to carry human beings.

For a real boat prepreg and nomex is way too expensive and will not offer a lot of advantages over more traditional building materials unless you want to compete in the America's Cup.

> I don't want the weight penalty of a gel coat if possible.

A boat needs to be able to swim in a medium with an approximate density of 1g/cm³. Gelcoat has a density of about 1.2g/cm³,  so there is no real weight/buoyancy penalty.

Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I don't want to be rude, 
But like brainfart is saying above, it's  kind of hard to build a boat with prepreg, unless you are building a very expensive yacht without a budget limit :p
you are also talking about infusing UD with the prepreg and so on, but the prepreg allready has the "perfect" resin to fiber ratio, so you wont be able to add more dry fabric to keep that 
"perfect" ratio. But you could find some UD prepregs if needed Smile 
make sure you know what you are doing before buying all the stuff and maybe start of with some smaller parts to understand the entire process.

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
c01df1sh - 11 Years Ago
brainfart - 11 Years Ago
matthieutje65 - 11 Years Ago
c01df1sh - 11 Years Ago
brainfart - 11 Years Ago
c01df1sh - 11 Years Ago
ChrisR - 11 Years Ago
matthieutje65 - 11 Years Ago
wozza - 11 Years Ago
c01df1sh - 11 Years Ago
brainfart - 11 Years Ago
wozza - 11 Years Ago
ChrisR - 11 Years Ago
wozza - 11 Years Ago
ChrisR - 11 Years Ago
wozza - 11 Years Ago
matthieutje65 - 11 Years Ago
wozza - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search