By c01df1sh - 10/18/2014 7:38:11 PM				
            
                      
            Hi,
  I am pondering a new boat build which will, in all eventuality, comprise making the hulls (it's a catamaran), foils, beams and maybe even a mast. I am pretty impressed with the Easy-preg option for an off the mould finish, ready for paint directly - I don't want the weight penalty of a gel coat if possible. The hulls would be a Nomex sandwich and I assume that this would be OK with a 215 gsm vari-preg layer (don't want to go to the 430 or would the experts recommend a resin layer? If so, where do I get this as there is nothing on the Easy Composites site that looks like it fits the bill. I'd like to work on a single vacuum / over cure rather than doing curing the layers individually.
  My second train of thought is how to incorporate UD layers in the vari-preg system. The cat's beams, foils and mast will be a UD dominated laminate, so I will need to work this out! Again, is there sufficient resin within the vari-preg backing layer to co-infuse UD layers, or again will a resin layer be required?
  Got to build an oven of course, but I'd like to get the construction resolved in my head at least. 
  Thanks for the great tutorials.
  Cheers
  Andy
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By wozza - 10/25/2014 7:15:44 AM				
            
                      
            So far there has been no mention of moulds. Making moulds of this size suitable for prepreg or infusion for that matter will be costly, especially given that your basement workshop prevents the use of polyester.
           
		 | 			
		 
	
	
						
		 	
		
	 |