Jemboe
Jemboe
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 4
Hi,
I'm looking to restore this carbon fibre exhaust shield.
My proposal is sand back the sand back the cracked gel/ resin coat and to reskin it with CF, finishing with epoxy top coat.
It needs to be reasonably temperature resistant.
Could i get this done with a starter kit?
Cheers
Attachments
Termi.JPG
(
854 views,
230.00 KB
)
Tags
ducati
epoxy
exhaust
repair
temperature
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Carbon Fibre Exhaust Shield Repair....
Jemboe
-
11 Years Ago
Yep, that could be done with a high temp skinning starter kit. You can even buy it with the same...
Dravis
-
11 Years Ago
Only thing to add is to conduct a postcure on the part to make sure the resin doesnt go soft on its...
Warren (Staff)
-
11 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search