davro
davro
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
Hi,
I finally got around to creating a mould for 1/10 scale touring car, so I thought I would share with you helpful people
I had a brand new body shell left over from me racing days.
This new body shell was the perfect candidate to take a mould from, and I also had quite a bit of Easy Composites
Uni Mould
System left over from a
previous project
So I had all the necessary goodies to create a 1/10 body shell mould!
And some spare time to make a mould and video with some royalty free music, good times
Easy Leased the table 2 coats
Easy Leased the body shell 3 coats
Uni-Mould Tooling Gelcoat 3 medium coats
Uni-Mould Coupling Coat (
100g Chopped Strand Mat
)
Uni-Mould Tooling Resin (
450g Chopped Strand Mat
)
Lots of gloves and plastic cups
Here is a video showing the making of the mould.
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Edited
11 Years Ago by
davro
Reply
Like
12
Reply
wozza
wozza
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Nice, shame about the little bit of bridging
I did a 1/5th touring car body some years back. I found running the feed spiral a full 360 around the flange and the vac outlet in the middle of the roof worked best. Some breather cloth under the vac connector stops print through onto the seen side.
Warren
Carbon
Copies Ltd
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
RC Car Touring Body 1/10 Scale
davro
-
11 Years Ago
looking good, thanks for sharing!
matthieutje65
-
11 Years Ago
Thanks Matthieu, First product was a success, bar a few issues mainly caused by the infusion...
davro
-
11 Years Ago
Nice, shame about the little bit of bridging :) I did a 1/5th touring car body some years back. I...
wozza
-
11 Years Ago
Thanks for the suggestion wozza I am going to layup another bodyshell with a Red Carbon Fibre 2/2...
davro
-
11 Years Ago
Fixed up the imperfection in the rear light then applied the first 2K clear coat, been a while since...
davro
-
11 Years Ago
I did something similar with the red and black twill :) https://www.youtube.com/watch?v=dn_xmEIiGQU...
matthieutje65
-
11 Years Ago
Stickers on and Clear Coat applied :) ) Finish spoiler ) Sand back with 3000 grit ) Polish...
davro
-
11 Years Ago
Post Reply
Like
12
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search