Making mould for complex shaped patter
Making mould for complex shaped patter
Post Reply
Like
5
Making mould for complex shaped patter
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
muxiamandy
muxiamandy
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 8,
Visits: 80
Hi everyone,
I am new to this forum; first I would like to say thank you for easycomposites and talkcomposites for all the tips and ideas you have shared.
Now, I want to make a mould for this blade. I am not sure where to put the parting line; and if I should make a 2,or 3 part mould.
Can anyone help?
Attachments
image.jpg
(
725 views,
75.00 KB
)
image.jpg
(
668 views,
72.00 KB
)
image.jpg
(
702 views,
1.00 MB
)
Tags
multiple part mould
Sharp edge
split mould
Reply
Like
5
Reply
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Pretty complex part for a fibreglass mould. Certainly doable, but it's going to be a lot of pieces. And when it comes to making the final part, if you aren't using pre-preg then you're going to have to lay them up separately. Which means bonding all the pieces together after they have cured. If it is just a project for learning then go for it, you'll learn a lot. But if you intend to use it for something that places it under anything more than very low loads, then it may be quite weak.
As for how to make the mould, I think brainfart is on the money. 2 parts for the blade, 3 parts for the base, perhaps 2 if the angles permit. If we are on the same page then I think you understand where to put the barriers, but I'm a little confused as to what "space between the blade and the base" you are talking about. I'll try to draw a quick picture as to how I would flange it.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Making mould for complex shaped patter
muxiamandy
-
11 Years Ago
Two molds for the blade, three molds for the bottom attachment thing. MAYBE this can be reduced to 4...
brainfart
-
11 Years Ago
I casted the pattern using a turbine blade, half of the base has been left out though; the base...
muxiamandy
-
11 Years Ago
That is a pretty complex part. What do you want to do with the mold? Laying up some fabric and...
brainfart
-
11 Years Ago
Oh yeah you said so already.
brainfart
-
11 Years Ago
In any case, I will have to join the moulds together. It is a part that has been lying around for...
muxiamandy
-
11 Years Ago
Pretty complex part for a fibreglass mould. Certainly doable, but it's going to be a lot of pieces....
Hanaldo
-
11 Years Ago
Going off your pictures, this is how I would do it. Can't see any reason to do the base in 3 parts...
Hanaldo
-
11 Years Ago
Can you please reattached your pictures Hanaldo? I can't seem to download them. My computer...
muxiamandy
-
11 Years Ago
Ah dammit. I hate trying to do this stuff from my phone. I'll fix the links as soon as I can get to...
Hanaldo
-
11 Years Ago
The blade is 350 mm by 150 mm and it tapers from 40 mm to 5 mm, so yeah, you right, it will be...
muxiamandy
-
11 Years Ago
A silicone mandrel is a nifty tool to use when you're wet laying. Basically you need your mould...
Hanaldo
-
11 Years Ago
Hanaldo, sorry for asking, any chance for those sketches? I think I got my blade split line correct;...
muxiamandy
-
11 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search