Hi

Please can I ask for some advice?

I have got a bad scuff on the carbon fork of my bike, I do not think there is any real damage but I just want something to give me peace of mind (I have had a fork crack on me before). So would anyone recommend either 

1/ Black Epoxy Repair Filler 100g Pack

or

2/ Epoxy Rapid Repair Resin 500g Pack

for this

Also please can someone give me a rough idea of the postage costs of each of these to the Netherlands?

Thanks for your time and patience
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
With Bike Frame repairs we always recommend getting a professional bike repairer at a bike shop or similar look at it.  Once its confirmed as just a gelcoat/lacquer repair then go ahead and you should be fine.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search