With Bike Frame repairs we always recommend getting a professional bike repairer at a bike shop or similar look at it.  Once its confirmed as just a gelcoat/lacquer repair then go ahead and you should be fine.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Looks like a minor gelcoat/surface chip-off ... I would really like a higher resolution close up picture to assess the damage ..  I can not tell if the laminate has been compressed and created some hairline cracks on either side of the "chip" or if it is just reflections ???

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
easilyConfused
easilyConfused
Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)
Group: Forum Members
Posts: 2, Visits: 4
Thanks for the reply, what do you think please? 

http://www.talkcomposites.com/Uploads/Images/e1e4aef9-4e4f-40bf-a622-ce0a.jpg
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
Post pictures.

If the laminate is damaged, then simply applying some epoxy is not good enough. It needs to be rebuild using proper techniques.
easilyConfused
easilyConfused
Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)
Group: Forum Members
Posts: 2, Visits: 4
Hi

Please can I ask for some advice?

I have got a bad scuff on the carbon fork of my bike, I do not think there is any real damage but I just want something to give me peace of mind (I have had a fork crack on me before). So would anyone recommend either 

1/ Black Epoxy Repair Filler 100g Pack

or

2/ Epoxy Rapid Repair Resin 500g Pack

for this

Also please can someone give me a rough idea of the postage costs of each of these to the Netherlands?

Thanks for your time and patience
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search