d21d3q
d21d3q
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 22
I am going to make kiteboard.
As core I have 8mm plywood and I want to cover it with fiberglass.
Question is if it may be possible to make it in one shot. I found video where is shown infusion of kiteboard but it is not told if it have been done with one shot.
https://www.youtube.com/watch?v=7NFdIi9CJ_M
With such small distances do I still need resin spreading mat?
Another question is if it is better to apply one thick layer of fiberglass or two thinner layers?
Tags
infusion
Edited
11 Years Ago by
d21d3q
Reply
Like
8
Reply
ChrisR
ChrisR
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
I would still drill holes in the board to allow the resin to pass through, belt and braces.
From that video, yes they are doing both sides at once but it was quite obvious that the infusion stack was going to stall! - I've never seen an infusion so slow!!!!
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Two sided infusion with wooden core
d21d3q
-
11 Years Ago
If you want to 2 side infuse then you will need to drill a bucket load of holes in the core to allow...
ChrisR
-
11 Years Ago
Even if I have: bag (spreading mat) peel ply fiberglass core firberglass peel ply (spreading mat)...
d21d3q
-
11 Years Ago
If you have infusion mesh top and bottom then it should be OK but you will need to take care with...
ChrisR
-
11 Years Ago
Before covering with fiberglass I will glue together two 4mm plywoods on rocker table to give shape...
d21d3q
-
11 Years Ago
I would still drill holes in the board to allow the resin to pass through, belt and braces. From...
ChrisR
-
11 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search