d21d3q
d21d3q
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 22
I am going to make kiteboard.
As core I have 8mm plywood and I want to cover it with fiberglass.
Question is if it may be possible to make it in one shot. I found video where is shown infusion of kiteboard but it is not told if it have been done with one shot.
https://www.youtube.com/watch?v=7NFdIi9CJ_M
With such small distances do I still need resin spreading mat?
Another question is if it is better to apply one thick layer of fiberglass or two thinner layers?
Tags
infusion
Edited
12 Years Ago by
d21d3q
Reply
Like
17
ChrisR
ChrisR
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
If you want to 2 side infuse then you will need to drill a bucket load of holes in the core to allow the resin to pass from top to bottom.
Reply
Like
16
d21d3q
d21d3q
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 22
Even if I have:
bag
(spreading mat)
peel ply
fiberglass
core
firberglass
peel ply
(spreading mat)
bag,
peel plies from both sides are attached together on sides and resin will be spreaded drom side to side?
I suppose that only problem might be that one side can be faster than other?
Reply
Like
16
ChrisR
ChrisR
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
If you have infusion mesh top and bottom then it should be OK but you will need to take care with inlet and outlet positions.
How are you going to get the rocker into the board doing it this way?
Reply
Like
14
d21d3q
d21d3q
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 22
Before covering with fiberglass I will glue together two 4mm plywoods on rocker table to give shape to it, then I will make stack like I described in previous post and place it on rocker table, but just to control if it keeps shape.
Reply
Like
17
ChrisR
ChrisR
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
I would still drill holes in the board to allow the resin to pass through, belt and braces.
From that video, yes they are doing both sides at once but it was quite obvious that the infusion stack was going to stall! - I've never seen an infusion so slow!!!!
Reply
Like
18
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
17
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search