bend polyester resin cast by applying heat ?


Author
Message
palace
palace
Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)
Group: Forum Members
Posts: 6, Visits: 41
Would it be possible to bend a 2 cm thick water clear polyester resin cast by applying heat ?

Would a hot air gun work ? If so, what temperature would be ideal ?
Edited 11 Years Ago by palace
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
might work, you'll need to try it, depends on how far you want to bend it... best would be to put it in an oven and check now and then if it starts to bend

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO