bend polyester resin cast by applying heat ?


Author
Message
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
2cm is quite thick. What kind of radius do you want to apply?

Polyester resin, once completely hardened, is a three-dimensional network of one gigantic molecule, not a thermoplastic bunch of linear molecules like most household plastics. The heating and bending will cause some damage to the material, it will create cracks and broken chemical bonds. If this damage is visible depends on how much you bend the material.
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
might work, you'll need to try it, depends on how far you want to bend it... best would be to put it in an oven and check now and then if it starts to bend

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




palace
palace
Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)
Group: Forum Members
Posts: 6, Visits: 41
Would it be possible to bend a 2 cm thick water clear polyester resin cast by applying heat ?

Would a hot air gun work ? If so, what temperature would be ideal ?
Edited 11 Years Ago by palace