I understand Lantor Soric SF is now available in black, will you be stocking this at EC in the near future? 

Regards

Marc
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Marc,

Yes, it's a new product from Lantor anounced at JEC. I'm sure it will be a very useful product and so we'll certainly be stocking it as soon as we can.

Best regards, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
r0bsk1
r0bsk1
Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)
Group: Forum Members
Posts: 38, Visits: 307
Hi Matt, any futher news on the black soric?
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Not yet I'm afraid. It seems it's not available to buy yet but I'll keep you posted and assure you that as soon as it is, we'll be stocking it.

Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Maybe a stupid question but can I ask what so special about that Black Lantor Soric?
Is it just for the cosmetic aspect? 
Why not just spray the white lantor with a black spraycan before lay-up?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




r0bsk1
r0bsk1
Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)Supreme Being (572 reputation)
Group: Forum Members
Posts: 38, Visits: 307
The cut edge of the white soric core will be white and would need to be refinished. Other alterantive is to line the edge pf the layup with CF to make up the thickness of the soric.
Edited 14 Years Ago by r0bsk1
Warren
Warren
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Administrators
Posts: 214, Visits: 783
Also the other cosmetic advantage is if you are using only one layer of fabric over the soric then in some areas it can be possible to see the white soric underneath whereever there is any tiny pull of the weave.  Ideally you shouldnt see any soric if your weave is perfect, however reality is seldom like that!