Talk Composites - The Forum for Advanced Composites

Black Lantor Soric SF Core

http://www.talkcomposites.com/Topic1257.aspx

By marc37i - 4/12/2012 10:40:05 PM

I understand Lantor Soric SF is now available in black, will you be stocking this at EC in the near future? 

Regards

Marc
By Warren - 7/5/2012 11:11:44 PM

Also the other cosmetic advantage is if you are using only one layer of fabric over the soric then in some areas it can be possible to see the white soric underneath whereever there is any tiny pull of the weave.  Ideally you shouldnt see any soric if your weave is perfect, however reality is seldom like that!