I have a crack on my front derailleur braze on on my carbon bike.  The crack is narrow and is not all the way through the braze on tab - on inspection it does not appear to be deep.  Unlike most bikes, the braze on is actually moulded as part of the frame and not riveted or bolted on - so a replacement is not an easy option.

I was considering repair options, and wondered if using your Black Epoxy Repair filler would suffice or of there was a better recommendation?

The tab holds the front derailleur onto the bike - so the stress of the derailleur moving the chain between chain rings is all it has to deal with.  It is an electronic shifter, so there aren't any additional forces from a cable that a mechanical shifter would cause.

Thanks
Steve
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Can you post some pictures of the damage? It sounds like some filler is all you need, but it could possibly be more extensive than that. 