Hallo ;-)

I am making Robot arms in composite and have until now Normal closed cell foam in 10 mm as core.
But my parts has shape as a tube and is made at one time, not to parts glued together, the part is a free form shape with many round shapes, so now I want to use a core material there is more easy to form and better for infusion.

Here is a link to se the parts http://youtu.be/8PXKaC6_uJY   The Black parts is Carbon but alittle dusty :-)

But what is best ?

A)

     Layer 1 : 600g Carbon

     Layer 2 : Soric SF 3mm

     Layer 3 : 600g Carbon

     Layer 4 : Soric SF 3mm

     Layer 5 : 600g Carbon

Or

B)

     Layer 1 : 600g Carbon

     Layer 2 : 600g Carbon

     Layer 3 : 3D CORE PET 10mm

     Layer 4 : 600g Carbon

     Layer 5 : 600g Carbon 

Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Take your pick really. I wasn't quite sure what part you're looking at making, but Soric is definitely the way to go if you've got a complex shape. The PET core can flex into shapes, but not so easy. It's more flexible rather than drape-able, compared to the Soric which is more like a heavy cloth. To be honest, I was left less than impressed with the thicker PET cores, but I also don't want to conclude that they are as poor as my crude testing found. 

Looking at your lay-ups, I think the PET core will be the better solution in terms of weight. 
Qumec
Qumec
Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)
Group: Forum Members
Posts: 7, Visits: 77
Hi Hanaldo

Tanks for your awnser 
webkit-fake-url://D6E895A8-6806-4E97-B28D-0E831271C915/imagejpeg
Here is a pic of the part 

Weight is not a Big problem for me what I want is the stiffness
Edited 12 Years Ago by Qumec