Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Equipment and Materials
»
Soric SF or 3D CORE PET ?
Soric SF or 3D CORE PET ?
Post Reply
Like
7
Soric SF or 3D CORE PET ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Qumec
Qumec
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 77
Hi Hanaldo
Tanks for your awnser
Here is a pic of the part
Weight is not a Big problem for me what I want is the stiffness
Edited
12 Years Ago by
Qumec
Reply
Like
7
Hanaldo
Hanaldo
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Take your pick really. I wasn't quite sure what part you're looking at making, but Soric is definitely the way to go if you've got a complex shape. The PET core can flex into shapes, but not so easy. It's more flexible rather than drape-able, compared to the Soric which is more like a heavy cloth. To be honest, I was left less than impressed with the thicker PET cores, but I also don't want to conclude that they are as poor as my crude testing found.
Looking at your lay-ups, I think the PET core will be the better solution in terms of weight.
Reply
Like
6
Qumec
Qumec
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 77
Hallo ;-)
I am making Robot arms in composite and have until now Normal closed cell foam in 10 mm as core.
But my parts has shape as a tube and is made at one time, not to parts glued together, the part is a free form shape with many round shapes, so now I want to use a core material there is more easy to form and better for infusion.
Here is a link to se the parts
http://youtu.be/8PXKaC6_uJY
The Black parts is Carbon but alittle dusty :-)
But what is best ?
A)
Layer 1 : 600g Carbon
Layer 2 : Soric SF 3mm
Layer 3 : 600g Carbon
Layer 4 : Soric SF 3mm
Layer 5 : 600g Carbon
Or
B)
Layer 1 : 600g Carbon
Layer 2 : 600g Carbon
Layer 3 : 3D CORE PET 10mm
Layer 4 : 600g Carbon
Layer 5 : 600g Carbon
Tags
3D CORE PET
core materials
soric
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search