How to project templates of carbon fiber for complicated surface?


How to project templates of carbon fiber for complicated surface?
Author
Message
rhcp89
rhcp89
Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)
Group: Forum Members
Posts: 5, Visits: 45
Hello,


I'm studying on technical university and my job is to project (to model) the way the carbon fiber has to be put in mould which will be the negative of car body. In brief, my work will be used to create a body of a car of composites.

The problem is that the car body must be made of aerodynamic ,continuous shapes (no low-radius edges) so when the composite will be put then the unwanted folds may appear or that fiber will have to be cut in some places. I have no such an opportunity to make mould first and then put fiber on it as a test and given this, determine the way the templates should look like experimentally . I have to do it the other way round- I have to predict the shape of these templates given the 3d cad model of car body first.


So I would like to know are there any books, articles, methods etc, which tell how to cut that carbon templates for a given surface? Maybe there some graphics  which say how to determine the shape of these templates or software(I could import 3d model there)?

Thank you,Raportuj ten post
Reply
rhcp89
rhcp89
Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)
Group: Forum Members
Posts: 5, Visits: 45
>Brainfart,

"You can use the CAD software to determine the length of surface lines, the middle of a part (your zero) and several polar coordinates and determine the absolute minimum size of fabrics based on this data."

I dont understand why should I determine the absolute minimum size of fabric. In fact I want to use the biggest piece of fabric until there appear first distortions.


"The cheapest way for good cutting patterns is an existing mold and newspapers, the most exact is probably some cheap glass cloth (twill or satin weave) laid into the mold and then stabilized with some tape."

I dont have such an opportunity to use an existing mould. I have to do it theoretically, on computer that well that can be used in reality later.