Hi,

I'm almost done with my bike-frame and I have painted the whole frame with 5 layers of resin.
It has dried in 48 hours and when I started to wet-sand it (using 400,600,800 and 1200) the surface is really dull.
Do you know why this is:
Is it poor sanding (I actually tested with only 1200 and it is still dull)? or has the resin not hardened yet?

As soon as I put water on the surface it is nice and shiny again, but when the water has dried, the dullness comes back.
Reply
brummelisa
brummelisa
Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)
Group: Forum Members
Posts: 20, Visits: 144
I included a part that I have wet-sanded.

As you can see, I haven't touched the CF-part in the middle so you can see the dull areas towards the edges.

Do you think this will go away when I clear-coat it? Or have I done something wrong?
Attachments
IMG_1939.JPG (688 views, 1.00 MB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search