I bought a carbon roof, overall condition is okay, just some minor set back that is not noticeable in a few feet.  Up close you can see 1 large crack on the side, and small ones all the around the roof.  My problem is the long crack, it seems like it has gone through all the way down to the carbon itself.  Is there a way to fill the crack?  Do you just sand it and hope the clear coat can get through or do I need resin?  How do you spray the clear?  Do you sand first, then buff, then respray the clear?  Here are some pics

LONG CRACK







Here's a sample of the crack that goes around the roof.  Seems like these are sandable then buffable





Here's a big crack but I believe weather trim will cover this part but might as well fix it.


Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
To be honest, for a new product i would be returning it.

simple cracks can be cosmetically filled with resin either by sanding back or flexing ans syringing fresh resin in, then sanding to match and polishing back up.

However you have lots and lots of cracks which is going to be many hours work.

Also any that have gone right through to the reverse as well, will have compromised the strength significantly meaning you would need to add additional reinforcement to replace the lost strength where the carbon has itself broken.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search