Coefficient of thermal expansion.


Author
Message
RussellE
RussellE
Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)
Group: Forum Members
Posts: 6, Visits: 20
I am hoping to use carbon fibre composite tube for the pendulum of a precision regulator clock.  I believe that the coefficient of thermal expansion of pulltruded carbon fibre composite is somewhere between 0.1 and 0.3 ppm /°C but wonder if you can give a more exact figure  for your tubes so that I can design a compensator.

Thanks in advance.

Edit:  The coefficient is I believe negative.
Edited 11 Years Ago by RussellE
Reply
RussellE
RussellE
Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)
Group: Forum Members
Posts: 6, Visits: 20
O.K. Thanks Warren.  I guess I'll just have to try it out and if it isn't good enough then make a compensator.

Russell.