Hi all,

Is it possible to use the epoxy catch can (https://www.easycomposites.co.uk/cp1-resin-infusion-catch-pot-small) as a degassing chamber? 
Reply
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I leave mine on full vacuum (pump running) for a couple of minutes.  I have found that its best to warm the two components separately prior to mixing and degassing.  If you do it cold then it foams up quite a bit.  Slightly warm and it just bubbles.